Greetings and thanks for your kindly information... my case the manufacturer recommend the Electrode E 9018 for capping, but material is IS 2062... that's way I have confused with this matter... I don't have WPSand PQR for this work... we have WPS & PQR for SA 106 Gr B and SA 335... but we can't use these WPS for above mentioned work?
Thanks & Best regards
Krishnasamy. M
Welding Inspector
Fize Al- Shammary Gen. Cont. Est.
Kingdom of Saudi Arabia.
Mob: +966 592823768
> Date: Thu, 6 Jan 2011 20:33:05 -0800
> Subject: [MW:9121] Re: WPS and PQR for P 1 material and P 5
> From: hindu.vikas@gmail.com
> To: materials-welding@googlegroups.com
>
> Dear Krishna,
> P-NO ,1, And material is is 2062 , so you done
> the root with E7018 OF 2.4mm, Welding Electrode and final caping with
> also same , but you have choice to done the final caping with 3.5mm
> welding rod, no need of E9018
>
>
>
> On Jan 5, 4:46 pm, "manpreet " <manpreetsi...@rediffmail.com> wrote:
> > Dear Krishna,Please explain your query in detail,if you are qualifying PQR then you can always choose different filler metals for different passes or If you have WPS which mention different filler metal for Cap, Also the title is vague "WPS and PQR for P 1 material and P 5", Please clarify.RegardsManpreet SinghOn Wed, 05 Jan 2011 16:59:32 +0530 Saamy wrote>Dear All !> Could you help me any one... We have IS 2062 material>for rail welding... the manufacturer recommend for E 7018 for root,>hot and filling and E9018 for capping on IS 2062... My Question is how>to allow E 9018 on IS 2062? Both electrodes have different A No...>That is essential variable... So please give advice...>>-- >To post to this group, send email to materials-welding@googlegroups.com>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com>For more options, visit this group's bolg athttp://materials-welding.blogspot.com/>Theviews expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment