Answer for que:1.PT for Bevels
Answer for que:2.Acid Etching Test Required.
 
Regards,
SURESH.

On Mon, Jan 10, 2011 at 4:37 AM, Idris Mohiuddin <idrismohi@gmail.com> wrote:
Dear Experts,
 
Please throw some light on the following query:
 
1. As per ASME Sec VIII Div 1, is any specific NDE required for SS vessels greater than 3/4 inch thickness?
 
2. As per ASME Sec VIII Div 1, After cutting back the cladding of a clad plate vessel, what test is required before welding an internal attachment?
 
Regards
 
MIM

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...