Re: [MW:9209] preheat calculation

Hello Martin,
 
If you want to be sure, follow below mentioned link.
 
Starting with your basemetal analysis, the critical hardness @ coolingtime dt800-500 will be calculated.
When you know the minimal acceptabel dt 800-500, you can calculate the minimal heat-input necessary to avoid cracks.
When you establish this heat-input you can check what combinations preheat / heat-input in your situation (process / wallthickness etc) are realistic.
 
Now, try to satisfy your clients requirements as well.
 
 
Good Luck,
 
 
2011/1/13 Martin Prad <martin_prad@hotmail.com>
Hi freinds,
 
How to calculate a preheat? Is the any mathematic formula for this?
 
kind regards,
 
Martin.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...