Hi Sujay,
As per sec.IX, SS welder is Qualified to weld the SDSS, nut you check with the client spec. also, bcz they will restrict this one.
Regards,
Mani.
--
Regards,
E.Subramanian
-- As per sec.IX, SS welder is Qualified to weld the SDSS, nut you check with the client spec. also, bcz they will restrict this one.
Regards,
Mani.
On Sun, Jan 16, 2011 at 2:46 PM, PBR <pbrerode@gmail.com> wrote:
Dear Sujay,As per to the base metal grouping (ASME SEC IX QW-423.1),F number grouping (QW-432) no changes and so no need of separate qualification, but check other essential variables regarding welder performance refer QW-416.With Regards,P.Balajirajan.-------Original Message-------Subject: [MW:9239] WQT for Duplex SS--Dear All,Welder is qualified in SS material,it required separately to be qualified for Duplex SS material.thanks and regards
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Regards,
E.Subramanian
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment