Monday, January 17, 2011

Re: [MW:9254] BRANCH 3/4" FROM 4" LINE LP STEAM

Dear Santosh Karnire,

With thanks for your explanations but as you see on subject of my mail, I mean this connection as branch connection ( 3/4"x 4" ).

I'm waiting for your valuable comments.


Best Regards,

On Sun, Jan 16, 2011 at 3:31 PM, Santosh Karnire <skarnire@permapipe.ae> wrote:

Dear Zarei,

 

Srinivasulu is correct , it is not advisable.

 

Reason being – There will be a drastic reduction(i.e from 4" to ¾" ), leading to sudden change in Pressure and velocity of the fluid being transmitted, leading to safety issue.

 

Gap as wide as 40mm on each side is too large to be filled up by welding and I doubt if it is commercially viable. Concentric Reducer is will more cheaper and will be easier to weld to the main pipe I.e 4inch.    

 

Best Regards,

Santosh Karnire
Purchase Engineer



P.O. Box 4988, Fujairah, United Arab Emirates. www.permapipe.ae
Tel   : +971 9 2282540 Ext: 139   |   
Fax    : +971 9 2282541
Cell  : +971 55 6471359              |   Email : skarnire@permapipe.ae

**** Setting the international standard for Pre-insulated Pipe for the District Cooling and Oil & Gas Industries.


This message, including any attachments, may contain confidential information & may also be legally privileged. The information contained in this e-mail message is intended only for the use of the rightful & intended addressee & must not be disclosed to any third party without express permission. If you are not the intended recipient, you are hereby notified that any distribution, copying, review, retransmission, dissemination or other use of this electronic transmission or the information contained in it is strictly prohibited. If this email is received in error, no confidentiality or privilege is waived or lost. Please notify the sender or email contactus@permapipe.ae & delete the email you have received from your system & destroy any hard copy.

From: Srinivasulu Kalasapati [mailto:nirgunaya@gmail.com]
Sent: Sunday, January 16, 2011 11:26 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:0] BRANCH 3/4" FROM 4" LINE LP STEAM

 

Usually it's not advisable to do that so.

On Sat, Jan 15, 2011 at 5:02 PM, ENAYAT ZAREI <zarei.enayat@gmail.com> wrote:

Dear All,

Is it possible to weld pipe 3/4" to pipe 4" in LP steam service  in the form of Pipe to Pipe (we have no any sockolet or Halfcoupling, ...)?

Does it need REINFOCEMENT?

your reply is highly appreciable.

 

Regards

Zarei

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Ohm Guru Namasivaya

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...