Hi Kisan,
 
As per ASME SEC IX QW 404.22 it is non essential variable. So you can use as it with insert.
Please read below given Clause.
If any doubt is in your mind feel free to call or mail me.
 
 

QW-404.22 The omission or addition of consumable

inserts. Qualification in a single-welded butt joint, with or

without consumable inserts, qualifies for fillet welds and

single-welded butt joints with backing or double-welded

butt joints. Consumable inserts that conform to SFA-5.30,

except that the chemical analysis of the insert conforms to

an analysis for any bare wire given in any SFA specification

or AWS Classification, shall be considered as having the

same F-Number as that bare wire as given in table QW-432.

Thanks & have a nice day

--
With Warm Regards,
Prakash Verma
Metallurgist -Drilling Riser Systems(Welding)
QS Supply Chain.
Aker Solutions Supply chain hub-India
AkerSolutions
Tel.+91-20-66 28 8538,09503021486
Email. prakash.verma@akersolutions.com

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kisan Gamane
Sent: Monday, January 17, 2011 11:22 AM
To: materials-welding@googlegroups.com
Subject: [MW:9254] WPS without consumable insert

Dear Expert
Please advice me about following.
 
If WPS ( GTAW)  is qualified for  without consumable  insert ; can we use it for with insert.
Code used for acceptance:- ASME sec IX
 
Thanks in advance for ur help.
 
Thanks & regards

--

 

किसन गामणे

नाशिक

After falling twice to conquer the mount

Everest, Edmund Hillary said-
I'll come again and conquer you because as a mountain you can't grow,
but as a human I can..."


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...