Tuesday, January 18, 2011

Re: [MW:9283] welder qualification from cs to ss and vice versa

Check ASME IX QW-400-450

On Tue, Jan 18, 2011 at 10:16 AM, krishna <wiqw@rediffmail.com> wrote:
dear all,
                     how a welder qualified in carbon steel can also weld stainless steel and vice versa?

my question is where in ASME sec ix it is given ?

pls clarify

regards,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
 
 
MANISH YADAV
8609649383,7877056928

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...