AS PER SECTION IX QW 423, IF ONE WELDER QUALIFIED IN CARBON STEEL THAT
IS P1 HE CAN WELD METALS P1 THROUGH P11, P34 AND P41 THROUGH P49. OK
STAINLESS STEEL P NO. IS P8 SO HE CAN WELD .





On Tue, 18 Jan 2011 12:27:35 +0530 wrote
>No he cannot weld on SS if qualified on carbon steel.With kind
regards,Vinod Kumar KatariaGM - OperationsBliss Anand Private
Limited,92B/93B Sector 5 IMT Manesar,Gurgaon,National Capital Region
Delhi.India .Phone : +91-124-4366000 (9 Lines)Mobile Phone : +91-
9560199004Fax : +91-124-2290884From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: Tuesday, January 18, 2011 10:17 AM
To: materialswelding
Subject: [MW:9281] welder qualification from cs to ss and vice
versadear all,
how a welder qualified in carbon steel can also weld stainless steel
and vice versa?

my question is where in ASME sec ix it is given ?

pls clarify

regards,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...