RE: [MW:9290] RE: 9281] welder qualification from cs to ss and vice versa

Hi All,
 
Mr. Vinod is right.Welder can weld CS to SS, but if he is using same F no & if he is qualified With F no 1
 he can weld with other F no without requalification.
 
 

--
With Warm Regards,
Prakash Verma
Metallurgist(Welding)-Drilling Riser Systems
QS Supply Chain.
Aker Solutions Supply chain hub-India
AkerSolutions
Tel.+91-20-66 28 8538,9503021486
Email. prakash.verma@akersolutions.com

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vijayakumar sivanandan
Sent: Tuesday, January 18, 2011 12:01 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9288] RE: 9281] welder qualification from cs to ss and vice versa

he can weld on ss when qualified with same FNo i.e  if a welder in CS qualified with FNo 6 filler wire for GTAW, He can weld SS with same FNo,But Vice versa can't be done as deletion of purging is an essential variable
 


 
On Tue, Jan 18, 2011 at 11:13 AM, Vinod Kataria <vinod.kataria@blissanand.com> wrote:

No he cannot weld on SS if qualified on carbon steel.

 

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: Tuesday, January 18, 2011 10:17 AM
To: materialswelding
Subject: [MW:9281] welder qualification from cs to ss and vice versa

 

dear all,
                     how a welder qualified in carbon steel can also weld stainless steel and vice versa?

my question is where in ASME sec ix it is given ?

pls clarify

regards,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...