Re: [MW:9295] Calibration of Welding m/c.

Dear PSP..
 
Welding machines calibration will directly releated to heat input -control measure.. Hence machine calibration is required to ensure the display of current & voltage.
 
br,
 
msms

On Tue, Jan 18, 2011 at 12:58 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear all,
Why we need to have calibration certificates of welding machines prior to start of fabrication activity?
As we can qualify WPS without the same.
Pl. reply.
Thanks & Regds,
PSP

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...