Hi
 
Since spec. clearly indicates the range, it has be to within the range, otherwise not acceptable
 
Thanks & Regards,
 
K. Babu

----- Original Message -----
Sent: Wednesday, January 19, 2011 11:47 AM
Subject: [MW:9317] Higher value of UTS, acceptable?

Dear all,
 
I have a material A350 LF2, CL1  with UTS of 724MPa (As mentioned in TC of Manufacturer).
 
As per ASME Sec IIA, requirement is 485 - 655 Mpa.
 
The higher value of UTS beyond the spec requirements is aceptable?
 
Thanks.
Regards,
JJ

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...