Dear Mr. Ali,

Is it standard or Non Standard type fitting ?

If the fittings is certified as per B 564, refer clause no. 6. It was mentioned that a little thickness reduced by grinding, what is quantum and location?

With Best Regards,

Jignesh R Rana
Manager - QA & QC
Linde Engineering India Pvt. Ltd.


This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.





ali asghari <asgharialigl@gmail.com>
Sent by: materials-welding@googlegroups.com

20/01/11 14:12

Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
Re: [MW:9347] RE: 9343] THICKNESS LOSS IN UNSO6625





Dear Mr.Bazrafshan
thank you for reply.
but in mentioned list, there is not suitable document.
regards

On Thu, Jan 20, 2011 at 11:30 AM, Bazrafshan,kazem <KBazrafshan@bpc.co.ir> wrote:
Dear Sir:

Please see referenced documents(Clause 2) in ASTM B564,I think these referenced STDs may be useful.

 

Regards

Bazrafshan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent:
Thursday, January 20, 2011 9:16 AM
To:
materials-welding@googlegroups.com
Subject:
[MW:9343] THICKNESS LOSS IN UNSO6625

 

Dear All

in some cases in UNS06625 fittings, alittle thickness reduced by grinding, now in which section of ASTM  i find the acceptance criteria of thickness loss?(i don't find in ASTM B564)

REGARDS

 

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...