Re: [MW:9398] Base metal range for repair qualification

Dear JJ,

Thanks for your confirmance, yes it is indeed a prject requirement else QW 202.3 would be applicable,

So, A repair PQR with 9.5mm thickness will serve the purpose, Thanks again.

Regards
Manpreet Singh




On Sat, 22 Jan 2011 03:10:37 +0530 joshi jaydeep wrote
>
Manpreet,
 
Refer QW 202.3 of ASME Sec IX:
 
You are on right path.
 
Moreover, you need not to have repair PQR unless it is project specific requirement. As per above mentioned clause, you can use any WPS which is quaified for fresh welding and meeting all your all other requirement.
 
Regards,
JJ
>

Jaydeep Joshi | Welding Engineer, TDW India Limited

Plot No 16 | Phase –III | Alindra – Savli G.I.D.C | Taluka : Savli | Vadodara – 391 775

Board : +91-2667- 619900 | Fax : +91- 2667- 619501| Extension : 7845

E-Mail : jaydeep.joshi@tdwilliamson.com  | www.tdwilliamson.com

Cell: +91 9978959626

P    Before printing, Think about ENVIRONMENTAL responsibility


>
On Fri, Jan 21, 2011 at 12:09 PM, manpreet <manpreetsin88@rediffmail.com> wrote:
>
Dear All,
>
>PQR "1434" with P1 Gr2 materials with 12.7mm base metal thickness,
>
>A repair PQR "1458" prepared with same materials for same 12.7mm base metal thickness, repair WPS "5799-10" for PQR 1458 have base metal thickness of 9.5mm,

>since Impact test is mandatory, base metal thickness limits shall be 12.7 to 25.4mm, which means WPS is not qualified, Please confirm my understanding.
>
>Regards
>Manpreet Singh 

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...