Thanks Amitabha,
As I know by AC welding oxygen pick up (Generally 160~200 ppm) during welding is quite less than DC welding (Generally 250~300 ppm) which gives you a better toughness property.
But, how the Oxygen pick up is less in AC welding?
Kindly explain mechanism of the same.
Regards,
Bhavesh Patel
On Fri, Jan 21, 2011 at 5:33 PM, amitabha.bhattacharya <amitabha.bhattacharya@bwgindia.com> wrote:
Hi Bhavesh,
You may expect higher toughness values with AC welding for CrMo-steels.
Thanks
Amitabha
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of JIGO
Sent: Friday, January 21, 2011 2:55 PM
To: Materials & Welding
Subject: [MW:9372] AC welding for P5A & P5C
Dear All,
Why we are using AC current for SAW welding in low alloy steel (Mainly
for P5A & P5C) ?
Kindly share your valuable input.
Regards,
Bhavesh Patel
ISGEC, Dahej
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment