Dear Mehta

 

Buttering weld is procedure to rectify wide gaps (root openings) greater than those permitted by AWS D11 (normally found in tubular joint in structural connection) and/or client specification, but not greater than 19 mm or twice the thickness of the thinner part, whichever is lesser. Procedure shall be qualified.

 

Fitya a



2011/1/25 B D Mehta <bdmehta.sap@isgec.com>

Dear All

 

Any body can explain me why we do buttering on weld edges of similar materials before welding .

 

Regards

B.D.Mehta

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...