Re: [MW:9469] RE: 9462] Electrode Vs WPS & PQR

in addition for CRO (overlay),  AWS classification an essential variable
ans some times in SAW process require same brand of wire/flux combination in API codes

On Tue, Jan 25, 2011 at 10:27 PM, John Henning <jhenning@deltak.com> wrote:
No it is not.  Code only requires same F number {QW-404.4} and, if
appropriate, A number {QW-404.5}.

Typically a customer requirement.

John

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of sn vl
Sent: Tuesday, January 25, 2011 8:36 AM
To: Materials & Welding
Subject: [MW:9462] Electrode Vs WPS & PQR

Hi..

It is Mandatory to USE the same electrode used in PQR , in Production
welds..

Regards
SN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...