Re: [MW:9470] Heat treatment in a Piping Joint as per ASME B31.3

Dear Yoganandhan,
 
I suppose the material is CS (P=1)
In that case, You are right, the PWHT will not be required as per the para 331.1.3. para 328.5.4 gives the governing thickness. If the thickness through weld is less than 40 mm, you need not carry out the PWHT.
 
I hope this clarifies,
 
With best regards,
 
Prasad JOSHI
Linde
 
On Tue, Jan 25, 2011 at 1:46 PM, yoga nandhan <yoganandhan@gmail.com> wrote:
Can anyone please clarify, whether heat treatment is required in a piping branch connection with joint thickness of 17 mm Header pipe with a connecting 22 mm thik weldolet(at joint).

As per Clause 328.5.4, i understood Heat treatment is not required

Please Clarify.

Thanks in advance

Yoganandhan.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...