Hi.

no problem just take Spot RT on + joint to ensure any weld crack or any
defects at intersection and found Ok release the joint. All codes
permits.



On Wed, 26 Jan 2011 10:06:34 +0530 wrote
>




Dears, we have a weld joint between elbows in wich the seams coincide.
>

>
How can we support this issue?, the restriction is only for pipes or
for elbows as well?
>

>
Thanks for your help.
>
>
>
Eduardo Calva
>
>
>

>


Date: Sat, 22 Jan 2011 04:59:12 +0000
>To: materials-welding@googlegroups.com
>Subject: [MW:9402] Painting requirement for Burried application
>From: manpreetsin88@rediffmail.com
>
>Dear All,
>
>Painting being carried out for buried installation, I have two queries
:-
>
>(1)- bonnet studs & nuts of top entry valves shall be protected from
blast cleaning?
>
>(2)- valve including bolting has to be completely painted in order to
ensure continuity of the coating?
>
>As a general engineering practice, I would say "YES", though some
advise from Painting experts would be much appreciated. Please confirm,
it's urgent...
>
>Regards
>Manpreet Singh
>

>--
>To post to this group, send email to materials-
welding@googlegroups.com
>To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...