 Dear K.V.S.Reddy
aws 5.28 is for  creep resistance high strenght low alloy steel consumbles  and 5.9 is for stainless steel consumbles.
thanks & regards
Chandrakant,



From: VENKATA SWAMI REDDY KARRI <kvsreddy777@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 23 January, 2011 4:44:12 PM
Subject: [MW:9412] sfa specification for ER 316L

Dear all,
 
 
previews project wps showing SFA NO AWS 5.28 for ER 316L But it is approved by client and PQR also stated that same as WPS. actually it is 5.9 as of my knowledge. Does anybody know any special thing there about 5.28 for ER316L

--
 

Best Regards,

K.V.S.Reddy,
Q.C.Inspector(Piping&Welding),
BS-132 Project,
SKEC Eng& Con Ltd.,
Postbox no-55653,
Sabahiya-54567,
Kuwait.
kvsreddy777@gmail.com,karryswamireddy@yahoo.com,
Ph:00965-94414396.
PleaseSave a tree. Don't print this e-mail unless it's really necessary
L

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...