Wednesday, January 26, 2011

Re: [MW:9494] impact test specimens

Dear Mr Reddy,
                       You have to take all the required CVN specimens at all the locations specified. 
@12 o'clock- WCL,FL, Fl+2 each 3 specimens
@3o'clock & 6o' clock also same.
This is taken to know the material properties at each position.


2011/1/26 VENKATA SWAMI REDDY KARRI <kvsreddy777@gmail.com>
Dear All,
 
Acording to our spec " Impact test sets shall be taken from 12 o'clock, 3 o'clock and 6 o' clock at
centre of weld
fusion line
+2mm from fusion line in the parent metal
 
Each test set shall include 3 specimens"
 
 
I have a doub't that we have to take the specimens  ex:   for centre of the weld 3specimens need to take at 12 o' clock  or 1 from 12,3and 6o'clock respectivly
 


--
 

Best Regards,

K.V.S.Reddy,
Q.C.Inspector(Piping&Welding),
BS-132 Project,
SKEC Eng& Con Ltd.,
Postbox no-55653,
Sabahiya-54567,
Kuwait.
kvsreddy777@gmail.com,karryswamireddy@yahoo.com,
Ph:00965-94414396.
PleaseSave a tree. Don't print this e-mail unless it's really necessary

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...