Wednesday, January 26, 2011

Re: [MW:9495] Welding query on super duplex pipe and fittings

No such restriction in B31.3, however you can be avoid it in case pipe to elbow (rotate the pipe). and in case of elbow to elbow just ensure that the welds are defect free. (you may ground flush the weld  and do 100% RT before joining them) 

On Wed, Jan 26, 2011 at 5:15 PM, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:
Dear team members,

The material spec is super duplex UNS 32760.
Construction code is ASME B31.3.
Operating pressure is 16Bar.
We have bought the elbows and pipe material with the logitudinal weld seam.
During the fabrication we have faced with the problem on elbow to elbow and pipe to elbow welding. The problem is the manufacture weld seams are in the same line as indicated in the attached photos. Is it acceptable?

Please share your experiences.

best regards,
Elshan.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...