Thursday, January 27, 2011

Re: [MW:9499] Purging Gas for Fillet Weld

Dear Yoga,

for GTAW welds, an internal 100% argon shall be used for the root pass and second layer (i.e. Hot Pass) of Stainless Steel Welds.

Regards
Manpreet Singh



On Wed, 26 Jan 2011 21:29:54 +0530 yoga nandhan wrote
>

>

Can anyone please clarify,  for Fillet weld to be carried outin a S.S Pipe (4.5mm wall thickness) to support joint with GTAW Process. Is itrequired to give Purging Gas in pipe.  (as per Clause 7.5 of API582. (attached)).

 

Pipe Material: SA312 TP316/316L

Support Material: SA240TP316/316L

 

Thickness: 4.5 mm Max.

 

Thanks in advance.


>

Best Regards,

YoganandhanPalaniappan

 

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...