Thursday, January 27, 2011

RE: [MW:9500] Weld seams coinciding

Thanks a lot, could you please give some code and clause?

Eduardo Calva



 



Date: Wed, 26 Jan 2011 11:00:40 +0000
To: materials-welding@googlegroups.com
Subject: Re: [MW:9488] Weld seams coinciding
From: muthu_barathi@rediffmail.com

Hi.

no problem just take Spot RT on + joint to ensure any weld crack or any
defects at intersection and found Ok release the joint. All codes
permits.



On Wed, 26 Jan 2011 10:06:34 +0530 wrote
>




Dears, we have a weld joint between elbows in wich the seams coincide.
>

>
How can we support this issue?, the restriction is only for pipes or
for elbows as well?
>

>
Thanks for your help.
>
>
>
Eduardo Calva
>
>
>

>


Date: Sat, 22 Jan 2011 04:59:12 +0000
>To: materials-welding@googlegroups.com
>Subject: [MW:9402] Painting requirement for Burried application
>From: manpreetsin88@rediffmail.com
>
>Dear All,
>
>Painting being carried out for buried installation, I have two queries
:-
>
>(1)- bonnet studs & nuts of top entry valves shall be protected from
blast cleaning?
>
>(2)- valve including bolting has to be completely painted in order to
ensure continuity of the coating?
>
>As a general engineering practice, I would say "YES", though some
advise from Painting experts would be much appreciated. Please confirm,
it's urgent...
>
>Regards
>Manpreet Singh
>

>--
>To post to this group, send email to materials-
welding@googlegroups.com
>To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...