Re: [MW:9501] Purging Gas for Fillet Weld

No need if it is a support welded on the pipe.But if u welded like end plate (groove+fillet) need.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 1/26/11, yoga nandhan <yoganandhan@gmail.com> wrote:

From: yoga nandhan <yoganandhan@gmail.com>
Subject: [MW:9489] Purging Gas for Fillet Weld
To: materials-welding@googlegroups.com
Date: Wednesday, January 26, 2011, 6:16 PM


Can anyone please clarify,  for Fillet weld to be carried out in a S.S Pipe (4.5mm wall thickness) to support joint with GTAW Process. Is it required to give Purging Gas in pipe.  (as per Clause 7.5 of API582. (attached)).

 

Pipe Material: SA312 TP316/316L

Support Material: SA240TP316/316L

 

Thickness: 4.5 mm Max.

 

Thanks in advance.


Best Regards,

Yoganandhan Palaniappan

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...