Re: [MW:9505] Purging Gas for Fillet Weld

Hi
 
I think NOT required for Fillet welds especially pipe to supports .
 
Suresh

On Thu, Jan 27, 2011 at 8:07 AM, Karthik <karthik6684@yahoo.com> wrote:
No need if it is a support welded on the pipe.But if u welded like end plate (groove+fillet) need.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 1/26/11, yoga nandhan <yoganandhan@gmail.com> wrote:

From: yoga nandhan <yoganandhan@gmail.com>
Subject: [MW:9489] Purging Gas for Fillet Weld
To: materials-welding@googlegroups.com
Date: Wednesday, January 26, 2011, 6:16 PM



Can anyone please clarify,  for Fillet weld to be carried out in a S.S Pipe (4.5mm wall thickness) to support joint with GTAW Process. Is it required to give Purging Gas in pipe.  (as per Clause 7.5 of API582. (attached)).

 

Pipe Material: SA312 TP316/316L

Support Material: SA240TP316/316L

 

Thickness: 4.5 mm Max.

 

Thanks in advance.


Best Regards,

Yoganandhan Palaniappan

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...