Re: [MW:9506] Welder qualification without/with backing

Hi,

If you are qualifying welder in accordance with ASME sec ix, Welder can weld with backing even if one is not qualified with backing, for Welder Qualification, Deletion of Backing is essential variable not addition of Backing.

Regards
Manpreet Singh



On Wed, Jan 26, 2011 at 4:32 PM, Fitria Rahman <t.chintaqa@gmail.com> wrote:
>

Hi expert


>

How a welderqualified in a single full penetration joint without backing can also weld in ajoint with backing (double V or U) and vice versa in SMAW process? Can you puta specific section?

 


>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...