Re: [MW:9507] impact test specimens

Dear Muhammed,

FL+5 is not mandatory and generally applicable for Cryogenic service (low temperature -100 deg), however there is no harm if you do it for normal service temperatures.

Regard
Manpreet Singh

 

On Thu, 27 Jan 2011 09:20:30 +0530 "Muhamad Zuhdey Sharifudin" wrote
>
>both are u are true...but need to combinetogether
>
>
>12 o'clock (weld metal, FL and FL+2, FL+5), 3 o'clock(weldmetal, FL and FL+2, FL+5) and 6 o' clock (weld metal, FL and FL+2, FL+5)
>
>
>
"manpreet " <manpreetsin88@rediffmail.com>
>Sent by: materials-welding@googlegroups.com

01/27/2011 11:07 AM

Please respond to
>materials-welding@googlegroups.com

>

To
"materials-welding " <materials-welding@googlegroups.com>
cc
Subject
Re: [MW:9501] impact test specimens

>

>

>
>
>Dear Reddy,
>
>Your spec means, for weld metal, FL and FL+2, impact test shall be carriedout for top, centre and root region, each of the test would require 3 specimens.
>
>let me know if you could interpret this correctly or else I would explainwith detailed sketch.
>
>Regards
>Manpreet Singh
>
>
>
>On Wed, 26 Jan 2011 13:29:53 +0530 VENKATA SWAMI REDDY KARRI wrote
>>

>Dear All,
>
>Acording to our spec " Impact test sets shall betaken from 12 o'clock, 3 o'clock and 6 o' clock at
>centre of weld
>fusion line
>+2mm from fusion line in the parent metal
>
>Each test set shall include 3 specimens"
>
>
>I have a doub't that we have to take the specimens ex: for centre of the weld 3specimens need to take at 12 o' clock or1 from 12,3and 6o'clock respectivly
>
>
>
>>--
>>

>

Best Regards,

K.V.S.Reddy,
>>Q.C.Inspector(Piping&Welding),
>>BS-132 Project,
>>SKEC Eng& Con Ltd.,
>>Postbox no-55653,
>>Sabahiya-54567,
>>Kuwait.
>>kvsreddy777@gmail.com,karryswamireddy@yahoo.com,
>>Ph:00965-94414396.

>PleaseSave a tree. Don't print this e-mailunless it's really necessary
>
>>

--
>>To post to this group, send email to materials-welding@googlegroups.com
>>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>>For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
>>The views expressed/exchnaged in this group are members personel viewsand meant for educational purposes only, Users must take their own decisionsw.r.t. applicable code/standard/contract documents.
>>

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel viewsand meant for educational purposes only, Users must take their own decisionsw.r.t. applicable code/standard/contract documents.

This electronic mail content and any accompanying attachments ("the Message") is intended only for the named addressee ("the Recipient") and may contain information that is confidential, privileged and/or proprietary to the Sime Darby group of companies ("Sime Darby") and/or protected under applicable laws. If you are not the intended Recipient, you are strictly prohibited from using, disseminating, forwarding and/or printing the Message. Please notify the sender immediately by return e-mail and permanently delete all copies of the Message. Sime Darby disclaims all liability for any error, loss or damage arising from the Message being infected by computer virus or other malicious software. Any views and/or opinions expressed in the Message are solely those of the author's and do not necessarily represent those of Sime Darby's.

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...