Thursday, January 27, 2011

RE: [MW:9508] Purging Gas for Fillet Weld

This clause is only for full pen welds but not fillet welds.


Date: Wed, 26 Jan 2011 15:16:24 +0400
Subject: [MW:9489] Purging Gas for Fillet Weld
From: yoganandhan@gmail.com
To: materials-welding@googlegroups.com


Can anyone please clarify,  for Fillet weld to be carried out in a S.S Pipe (4.5mm wall thickness) to support joint with GTAW Process. Is it required to give Purging Gas in pipe.  (as per Clause 7.5 of API582. (attached)).

 

Pipe Material: SA312 TP316/316L

Support Material: SA240TP316/316L

 

Thickness: 4.5 mm Max.

 

Thanks in advance.


Best Regards,

Yoganandhan Palaniappan

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...