Thursday, January 27, 2011

Re: [MW:9509] Use of A 234 WPB in the place of A420 Gr.WPL6

Dear Thiru,

Completely agree with A. Pravean, also would like to add few points that A234 WPB is not good choice for -45 deg, usually limited upto -20 deg, A420 WPL6 is a perfect choice at this temp., with this material used as fitting, A333 Gr.6 is a good choice for piping.

Regards
Manpreet Singh



On Wed, 26 Jan 2011 09:45:13 +0530 praveen alavandar wrote
>Dear Thiru,
>
>Your were right.
>
>Assuming your service to be B31.3, A234 Gr.WPB will be a material classified under curve B of Fig.323.2.2 A of ASME B31.3
>
>Looking at your service condition (Design minimum -45 Deg.) this material cannot be used for the said service.
>
>You need to use A 420 WPL6 for your service.
>
>Regards,
>
>A.Praveen
>Welding Engineer
>Muscat
>
>--- On Tue, 1/25/11, thiru sam <thiruvenkatam_be@yahoo.co.in> wrote:
>
>> From: thiru sam <thiruvenkatam_be@yahoo.co.in>
>> Subject: [MW:9459] Use of A 234 WPB in the place of A420 Gr.WPL6
>> To: "Materials & Welding" <materials-welding@googlegroups.com>
>> Date: Tuesday, January 25, 2011, 7:16 PM
>> Dear All,
>>
>> Can somebody advice me about the use of A234 WPB
>> fittings in the
>> place of A420 Gr.WPL6 for the LPG line.
>>
>> I hope,A234 WPB is for medium and elevated
>> temperatures,whereas A420
>> is for lower operating temperatures. and moreover A420 is
>> having
>> impact test properties.
>>
>> So i hope we cant use the A234 WPB in place of A420,even
>> though
>> tensile properties are same.
>>
>> In my project,Design Temperature of LPG line is -45 deg to
>> +85 deg.
>>
>> Is my statement is correct?
>>
>>
>> Regards,
>>
>>
>> Thiru.
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members
>> personel views and meant for educational purposes only,
>> Users must take their own decisions w.r.t. applicable
>> code/standard/contract documents.
>>
>
>
>
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...