Dear Sadique

The joint sketch which you have shown is a double bevel groove + fillet joint.

In order to know the fusion of plate A with plate B, you have to use a normal beam probe and scan from the back of Plate A if accessible.

What are the plate thicknesses ??

Regards

Prem Nautiyal

On Mon, 03 Jan 2011 16:36:24 +0530 wrote
>Actually I want to know the defect of incomplete fusion in T-joint

fillet weld.Please see attached Drawing for reference. In that Can we

know about fusion on plate A with welding with angle probe or we must

need TR probe to identify the defect? Bevel angle side fusion we get

with angle probe.


On Mon, Jan 3, 2011 at 2:51 PM, muthusrinivasan muthuselvam

wrote:

> Dear Mr.Sadique..

>

> what you are looking exactly in fillet weld UT..

>

> Can you elaborate little bit..

>

> br,

> msms

>

> On Mon, Jan 3, 2011 at 1:40 PM, Sadique Sheikh wrote:

>>

>> Dear All,

>> During UT inspection of fillet weld, Does we need both angle probe and

>> normal or TR probe?

>>

>> Thanks & Regards,

>> Mohd. Sadique Sheikh

>>

>> --

>> To post to this group, send email to materials-welding@googlegroups.com

>> To unsubscribe from this group, send email to

>> materials-welding+unsubscribe@googlegroups.com

>> For more options, visit this group's bolg at

>> http://materials-welding.blogspot.com/

>> The views expressed/exchnaged in this group are members personel views and

>> meant for educational purposes only, Users must take their own decisions

>> w.r.t. applicable code/standard/contract documents.

>

> --

> To post to this group, send email to materials-welding@googlegroups.com

> To unsubscribe from this group, send email to

> materials-welding+unsubscribe@googlegroups.com

> For more options, visit this group's bolg at

> http://materials-welding.blogspot.com/

> The views expressed/exchnaged in this group are members personel views and

> meant for educational purposes only, Users must take their own decisions

> w.r.t. applicable code/standard/contract documents.

>



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...