Wednesday, April 3, 2013

[MW:17280] Re: Test subsea welded-in valve seal

We had Nuke machinists that would do a "Blue Check" of the valve and seat surface after we did nuclear valve replacements.
Google: blue check a valve using Prussian Blue
It is a very accurate way to get a visual representation that the valve and seating surface are still perfect.
RESEARCH how to do it. If you don't know what your doing, you can get a false reading showing good, when in reality it is a bad seat but you did the test incorrectly.
Bob


On Sunday, March 31, 2013 6:55:02 PM UTC-7, toanvnguyen wrote:
Dear Experts,

We're doing a PLEM and TPAM project. The type of valves's welded-in valve. In spec. require as follow: "After fabrication's complete, welded-in valves shall be subject to seal tests in accordance with the relevant project valve specification to demonstrate the valve functionality has not been impaired during fabrication".
Could you pls give me some advice about this kind of tests. Many thanks.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...