Thursday, April 11, 2013

[MW:17347] RE: 17336] Request to provide filler metal & Flux combination for SAW process for low temperature service with Heat treatment

See Below _

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Aly
Sent: Wednesday, April 10, 2013 11:25 AM
To: materials-welding@googlegroups.com
Subject: [MW:17336] Request to provide filler metal & Flux combination for SAW process for low temperature service with Heat treatment

 

Dear Experts,

We are going to qualify welding procedure of following details

 

1.       Welding with

·         GTAW with ER70S2

·         SMAW with E7018-1 &

·         SAW

 

2.    Heat treatment after welding at 620°C @ 200min

3.    Impact testing after heat treatment at -46°C

 

Kindly  advise on  filler metal & Flux combination for SAW process to achieve impact properties after heat treatment.  I use the following for impact qualified welding;  ESAB Spool Arc 71 wire and ESAB OK 10.72 flux  - this combination is classified as F7P5-EM14K.   Although the petro-chems have, across the board, heartburn - using a combination with a deposited weld metal  manganese above the Sc .IX  A1 chemistry limit of 1.60% will give you superior impacts after PWHT. 

 

Can F7A8 EM12K  will this serve the purpose…!! Unknown – the combination (whatever it is) is classified only as welded (hence the ”A”) The response of this metal after the PWHT has not been tested.      

 

 

Thanks & regards

 

Ali Mhaskar,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...