Dear Experts ,
Weldolet ( Drain point ) is overlapping Long seam of 48 inch 90 deg LR Elbow ..
Design pressure : 96 Bar
Design temp ( Max/Min) : 80/5 deg C
Hydrotest Pressure : 120 Bar
NDT : 100 % RT , MPI
Application : Subsea
Service: Offshore Non Sour, Non Corrosive , HC Crude Blended Oil
Spec : ASME B 31.4
Elbow Spec: ASTM A 860 WPHY 65 WLDD
Kindly refer attached snap ..
My Question is what should be the NDT to be performed before & after welding of weldolet ? please put code/client reference .. ( Any )
( Kindly let me know if more information is required)
Thanks & regards.
ABHISHEK GHOSH
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment