Sunday, April 28, 2013

[MW:17579] Pre heat requirements for tack welding in P91

Dear Experts,

 

Regarding the subject mentioned, kindly clarify my following doubts.

(a)    Preheating required for P91 as per B 31.1 is 200°C (mini). Does it mean that this Pre heat shall be given for tacking also.

(b)   PWHT holding time for P91 mentioned in B 31.1 is 1 hr/25 mm; minimum 30 minutes. Does it mean that if the thickness is 6/10/12.5 mm the holding time is 30 minutes & for 15 ,20,30,40 mm the holding time is 36  48,72,96 minutes respectively.

(c)    I got some special heating curves for P 91 from our group. But Kindly explain about the reference /standard used for preparation of this heat curve ( eg- why the preheat maintenance is 4 hours & again free cooling).

 

S.Binoy

 

 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...