Hi, Siva, My apologies, In my earlier reply I should have added L suffix to the E316-16, there is a difference between E316-16 and E316L-16 as the carbon content varies, unless the electrode supplier dual certifies the electrodes as E316-16/E316L-16.
 
Hope the info clarifies.
 
 

From: siva subramanian <ian_siv@yahoo.co.in>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, 1 April 2013, 23:01
Subject: [MW:17261] Welding of E316L material -Reg

Dear sirs,
                 I have one clarification regarding welding of SA240 GR 316L material.
May I use E316-16 to weld 316L material.If it is not possible means What is reason behind?

Please Clarify me.

Always Thankful,
A.Sivasubramanian
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...