On Wed, Apr 3, 2013 at 2:53 PM, <mohdfirdaus.abdrahim77@gmail.com> wrote:
Ramesh,Actually I have the complete procedure for HDPE Pipe underground work. From the details procedure we can create the ITP. HDPE Pipe usually use fusion method either butt fusion or electro fusion. Can you give me jointing method for your work?. Details material use, PN number, size & thickness, product name. I'll try my best to help you.Firdaus,Refrain from commenting if you don't have the correct information, yes there are WPS for HDPE pipe.Ramesh,Inbox me a request and I will send you a copy.Cheers
From: mohdfirdaus.abdrahim77@gmail.com
Sent: Tue, 02 Apr 2013 09:32:54
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Cc: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Subject: Re: [MW:17268] HDPE Pipe INSTALLAITION ITP&WPSWPS?. I think there is no need for WPS. 2 type of fusion, electro fusion & butt fusion. It better you google it first before asking. Trust me, you'll find the solution when you google it. I found there too.
Mohd Firdaus Abd RahimQA/QCSent from my iPhone----Dear all,Any one can send HDPE PIPE under ground piping ITP &WPS FORMATThanksRAMESH
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Get your own FREE website and domain with business email solutions, click here--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
Best Regard,
Mohd Firdaus Bin Abd Rahim --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment