RE: [MW:17334] Pipe joint resting on the beam

The pipe needs a “shoe” to prevent corrosion down the road…good luck!

 

Mark Weaver

UOP Callidus

918.523.2273 O

918.549.8354 C

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sumod s
Sent: Wednesday, April 10, 2013 4:55 AM
To: materials-welding@googlegroups.com
Subject: [MW:17330] Pipe joint resting on the beam

 

sir,

 

Please explain the basic reason for not permitting the practice as seen in attached photo.

 

sumod

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...