Re: [MW:17371] Austinitic Stainless steel piping, corrosion environnement

it is not recommended to use  (304L & 316L ) at maritime environment.
(304L & 316L ) decrease chance of  sensitization  formation due to low carbon content. (OK)
but at maritime environment there are A very big danger called stress corrosion cracking ( SCC ) occurs at austenitic stainless steel .
it's recommended to use  super duplex alloy such as 2507; which resist ( SCC).


On Fri, Apr 12, 2013 at 8:26 PM, Ranendra Chakraborty <ranendrac6@gmail.com> wrote:
Dear Ghrab,
Check with API 571.

Regards,
Ranendra
On Fri, Apr 12, 2013 at 9:52 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:

Dear experts,

  Need your help.

Need to confirm if we can use austinitic stainless steel piping (A312 304L & 316L grades)  for maritime environnent and any risk of corrosion.

To code/standard i can refer ?

Regards.

-----
زكرياء غراب
GHRAB Zakaria
Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...