ASME IX 20012, QW 253, specifies the only essential variable in terms of filler metals as F& A numbers
& the diameters,the classification is regarded as non-essential variable, Please check your WPS and determine what electrodes was specified, and then contact the electrodes manufacturer and get support whether use of E7018 instead of E-7018-1 is acceptable and will not affect the welded joint's integrity.
Very Best Regards
Behrooz Alavi
From: Raghuram Bathula <raghurambathula@gmail.com>
To: Materials-Welding <materials-welding@googlegroups.com>
Sent: Sunday, April 14, 2013 1:19 PM
Subject: Re: [MW:17386] E 7018 used instead of E7018-1
To: Materials-Welding <materials-welding@googlegroups.com>
Sent: Sunday, April 14, 2013 1:19 PM
Subject: Re: [MW:17386] E 7018 used instead of E7018-1
what is the MDMT? there is no NDT. may be you can cut few welds to do CVN impact @ MDMT and convince your client.
or run a test coupon with E7018 and do impact testing at MDMT.
On Sun, Apr 14, 2013 at 3:41 PM, Binu Nair <binugnair1984@gmail.com> wrote:
Dear Experts,Our welders are used E7018 instead of 7018-1 for A333 Gr-6.Now client is asking to cut the joints.Moreover they are asking to prove the remaining joints whether they are welded with 7018-1 or not.Can anybody suggest a suitable method such as any NDT to prove that ?So please send your valuable suggestion with reference to code.Thanks & regards,Binu.--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment