Dear Experts
We wanted to use SA516 Gr70 plate from DANSTEEL (MTCs' are attached) where original marking on plate is as follows
UR
LR EH36 S355K2+N CE; refer the attachment
(SA516 65/70MTLTV is not punched on plate; but the marking on plate is traceable to given mtc…
Mtc shows Specification as ASME SA516 65/70 LR EH36 S355K2+N
Mill has issued letter regarding modification of marking as ASME SA561 65/70 MT LTV…(refer attachment)
We internally released these plates as marking on plate is traceable to MTC…further there is letter from Mill regarding the marking.
Kindly advise can we use this plate for ASME U Stamped Pressure vessel job
Ali
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment