Hi,
In my opinion No. this clause is for plates that is purchased offcut or Coil.
However I would like to point out, the MTC states ASME SA516. 65/70, but does not confirm the edition that it has followed to produce the plate. Isnt this a point of concern? Please read 19.1 of SA 20.
I definitely feel experts will share more on this.
From: Mhaskar Aly <mhaskar.aly@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, 16 April 2013, 16:00
Subject: Re: [MW:17432] SA516 Gr70 plates having different markings are acceptable for ASME ustamped Pressure Vessel
To: materials-welding@googlegroups.com
Sent: Tuesday, 16 April 2013, 16:00
Subject: Re: [MW:17432] SA516 Gr70 plates having different markings are acceptable for ASME ustamped Pressure Vessel
Dear friend,
Thank you for your advise...
Can following clause of SA20 will work...
13.4 Subdivided Plates:
13.4.1
By agreement between the purchaser and the
manufacturer or processor, each subdivided plate (a plate
separated from a master plate) shall be legibly marked with
the name, brand, or trademark of the organization that
subdivided the plate plus a code traceable to the required
markings, provided that the information required in 13.1,
cross referenced to that code, is furnished with the plates.
Thanks
Ali
On Tue, Apr 16, 2013 at 10:47 AM, rudolf saldanha <rudolf_jude@yahoo.com> wrote:
--Hi,Not an expert at all but just my 2 cents.Sec II, SA 20 - 13 clearly states the required markings. The key words are "SHALL". If this job is for audit purpose, I will definitely not go for it. But if it is a regular production the AI's approval may be sought. Finally the onus is on the manufacturer as far as the integrity of the vessel is concerned.
From: Mhaskar Aly <mhaskar.aly@gmail.com>
To: materials-welding@googlegroups.com
Cc: ali.m@velath.com
Sent: Tuesday, 16 April 2013, 13:04
Subject: [MW:17424] SA516 Gr70 plates having different markings are acceptable for ASME ustamped Pressure Vessel
--Dear ExpertsWe wanted to use SA516 Gr70 plate from DANSTEEL (MTCs' are attached) where original marking on plate is as followsURLR EH36 S355K2+N CE; refer the attachment(SA516 65/70MTLTV is not punched on plate; but the marking on plate is traceable to given mtc…Mtc shows Specification as ASME SA516 65/70 LR EH36 S355K2+NMill has issued letter regarding modification of marking as ASME SA561 65/70 MT LTV…(refer attachment)We internally released these plates as marking on plate is traceable to MTC…further there is letter from Mill regarding the marking.Kindly advise can we use this plate for ASME U Stamped Pressure vessel jobAli
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment