Re: [MW:17448] Invidual WPS from combined PQR

Yes you can make SMAW with Backing, OR only GTAW or GTAW+SMAW


From: sumod s <sumod.sadhupuram@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, 16 April 2013, 18:15
Subject: [MW:17440] Invidual WPS from combined PQR

Dear,
 
I have a PQR for GTAW +SMAW. Can i make seperate WPS for GTAW and SMAW(with backing) from this PQR. (with in all limits of thickness)
 
Sumod
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...