Saturday, April 20, 2013

Re: [MW:17489] Re: Radiography aerospace M250 welds

Dear sir,

                      D4 would be more suitable which is slow and reveal tiny discontinuities more visible and may be required longer exposure time needed  than for D2 .

regards
Kichu


From: SV Swamy <svswamy@gmail.com>
To: materials-welding@googlegroups.com
Cc: krm_ananthanarayanan@vssc.gov.in
Sent: Saturday, 20 April 2013, 12:08:26
Subject: [MW:17477] Re: Radiography aerospace M250 welds

If I remember right D2 is a slower finer grained film. Thus it may show some fine indications missed by D4. You can switch to D2 but you may find such indications and would have a problem deciding whether to leave them alone (and monitor them later in service if possible) or repair them. Repair may sometimes worsen and introduce more discontinuities. 

Better discuss with designer if possible before switching. 

Swamy
Retd. QA Metallurgist
Nuclear Fuel Complex, Hyderabad

On Friday, April 19, 2013 12:10:35 PM UTC+5:30, Mohanananthanarayanan KR wrote:
Dear all,

As per specification we have D4 film to be used for radiography of 7.8mm welds
of M250.As an investigation of a defect in UT D2 film was used and it detected
faint indications. The sensitivity IQI is seen in both the films as per
specification. Should we change to D2 film?

Regards

Ananthanarayanan
Trivandrum



**Print this e-mail only if absolutely necessary. Save paper and keep India Green**

***The information contained in this e-mail message and / or attachments to it may contain confidential or privileged information. If you are not the intended recipient and received this e-mail in error, please notify us by reply e-mail / telephone and  delete the message and attachments permanently. Thank you.***

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...