Re: [MW:17491] Welder validity

If the welder has been Qualified by the Manufacturer, yes he can work for y contractor without requalification. Else he need to qualify.
 
Thanks & Regards

J.Gerald Jayakumar
00968-99438165
From: Maulik Thakkar <mlkthakkar2@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Saturday, April 20, 2013 7:55 PM
Subject: [MW:17489] Welder validity

Dear all,
Query- one qualified welder under x contractor at one manufacturer. Now consider he left the x contractor & join y contractor & working under same manufacturer but at different location.
In view of above case is he qualified to do welding under y contractor at same manufacturer located at different place?......or need requalification?
Regards,
MHT
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...