RE: [MW:17565] Use of other brands of filler & Flux combination for SAW welding than what brand used during PQR


Dear Mr.Ali
 
Yes we can.
Please refer below
 

QW-404.33 A change in the filler metal classification

within an SFA specification, or, if not conforming to a

filler metal classification within an SFA specification, a

change in the manufacturer's trade name for the filler metal.
 

QW-254

WELDING VARIABLES PROCEDURE SPECIFICATIONS (WPS)

Submerged-Arc Welding (SAW)

QW-404.33 - Classification  - is coming under Nonessential variables

 

 
Regards
K.Govindan
 
 

Date: Fri, 26 Apr 2013 11:21:41 +0400
From: mhaskar.aly@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:17560] Use of other brands of filler & Flux combination for SAW welding than what brand used during PQR

Dear Friends
 
We have PQR with F7A8 EM12K from ESAB Brand ;
 
Can we use F7A8 EM12K from other Brands viz Bohler, Lincoln, Kiswel etc...
 
Is it acceptable as per SEC IX...
 
 
Ali Mhaskar
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...