Hi friends ,

Can anybody suggest better way to attach thermocouple on P91 pipe for SR avoiding the welding, in non- calibrated furnace? Metal temperature to be measured directly.

 

Ravinder Sharma

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...