Thursday, August 26, 2010

RE: [MW:6725] Charpy impact Test qulaification for an existing PQR

SS316L doesn't require CVN impact at -70 °C acc to B31.3 unless contract specifically request for it, in addition refer note 6 of table A-1 and note 3 of table 323.2.2


From: Larry [mailto:quality@unieng.com.au]
Sent: Thursday, August 26, 2010 9:13 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:6722] Charpy impact Test qulaification for an existing PQR

Hi there,

 

Material:  SS 316L

Thickness range: 4.8mm to 25.4mm

Code of Construction: ASME B31.3

 

 

Cheers,

 

Larry Zarate

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Thursday, 26 August 2010 1:03 PM
To: 'materials-welding@googlegroups.com'
Subject: RE: [MW:6722] Charpy impact Test qulaification for an existing PQR

 

what is your material, job thickness range and code of construction?

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: Thursday, August 26, 2010 5:31 AM
To: materials-welding@googlegroups.com
Subject: [MW:6716] Charpy Test

Hi There,

 

We have an existing WPS, The existing WPS doesn't have a cold service specification, and we would like to do a test coupon from that WPS and have it charpy tested, so we can revised the existing WPS. Now the requirement of the client is -70 degrees Celsius. Is that alright or do we have to do another PQR? Code is ASME IX.

 

 

Thank you,

 

Larry Zarate



No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...