Thursday, August 26, 2010

Re: [MW:6729] Charpy Test

You have to do an other PQR and register all supplementary essential parameters.

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for "Larry" <quality@unieng.com.au>"Larry" <quality@unieng.com.au>


          "Larry" <quality@unieng.com.au>
          Sent by: materials-welding@googlegroups.com

          26/08/2010 03:01

          Please respond to
          materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc


Subject

[MW:6716] Charpy Test

Ref


Hi There,

We have an existing WPS, The existing WPS doesn't have a cold service specification, and we would like to do a test coupon from that WPS and have it charpy tested, so we can revised the existing WPS. Now the requirement of the client is -70 degrees Celsius. Is that alright or do we have to do another PQR? Code is ASME IX.


Thank you,

Larry Zarate

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...