Dear Kisan,


Generally thinning will be in range of 4-12% depending on many factors / variables (such as - Forming method/ Process and machinery used, thickness of plate, Material type and grade, diameter of blank, etc).

Regards.
CK

 On 27 August 2010 15:55, Kisan Gamane <kisankrishna1506@gmail.com> wrote:
Dear all
Anybody can tell me about how many percentage thicness will be gets thin in ellipsoidal dish end?

--
Thanks & regards
Kisan Gamane
 
ॐ सर्वे भवन्तु सुखिनः, सर्वे सन्तु  निरामयः
सर्वे  भद्राणि  पश्यन्तु, मा कश्चिद दुखभाग भवेत्.
May all be happy. May all enjoy health and freedom from disease.
May all have prosperity and good luck. May none suffer or fall on evil days.
++++



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...