[MW:9565] AW: 9557] welding consumable for 34 CrMoNi6 material

Hi Dinesh,

 

This steel is difficult to weld.

Welding consumable: E80T5-B2-MH4 / Welding Alloys product: ROBOFIL B CrMo1 (FCAW)

If you need coated electrodes please refer.

best regards / mit freundlichen Grüßen

Siegbert Hafenscherer, Eng, IWE

Key Industry Manager (Strategic Industries)

 

Welding Alloys Group

 

Tel.:      +33 389786300

Fax:      +33 389786333

Mobil:   +49 173 9664991

 

E-Mail: siegbert.hafenscherer@welding-alloys.com

Web:    www.welding-alloys.com

 

Enclosed please find detail from data sheet from steel V124SC

 

Welding

Welding presents pro blems.

At any rate, parts should be wel ded in the

quen ched and tem pe red con di ti on.

Strength pro perties of the joint will not in all

ins tan ces come up to the va lu es of the

quen ched and tem pered base me tal.

The fol lo wing re com men da tions should be

followed: Pre he at to 300 - 400°C.

Temper af ter wel ding to about 30 - 50°C be -

low the tem pe ring tem perature re com men -

ded for the steel.

For ad vi ce in con nec ti on with dif ficult weld -

ments, plea se con sult our wel ding en gi -

neers or our Wel ding Tech no lo gy De part -

ment at Kap fen berg works.

 

Von: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Im Auftrag von DINESH TIWARI
Gesendet: Sonntag, 30. Januar 2011 11:52
An: welding groiup
Betreff: [MW:9557] welding consumable for 34 CrMoNi6 material

 

Hi Guys ,

We have to weld A36 grade material with 34 NiCrMo6 , can anybody tell me which electrode can be used for the same .
If somebody has welding parameters also then please share .


Best Regards ,

-----------------
Dinesh Tiwari

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...